AMS-QQ-A-250_28B
Aluminum Alloy, 7011 Alclad 7178 Plate and Sheet
Aluminum Alloy, 7011 Alclad 7178 Plate and Sheet
2012-09-01
有效
【范围】 1.1 Scope: This specification covers the specific requirements for 7178 aluminum alloy, 7011 alclad, plate and sheet; the general requirements are covered in AMS-QQ-A-250. The plate and sheet covered by this specification shall be an integral composite product consisting of a heat-treatable 7178 aluminum alloy core with thin layers of a 7011 aluminum alloy anodic to the core and of approximately equal thickness, bonded to both surfaces. 1.2 Classification: 1.2.1 Tempers: The plate and sheet are classified in one of the following tempers as specified (See 6.2): O T6, T62, T651 T76, T7651, or F temper (See 6.3). Definitions of these tempers are specified in AMS-QQ-A-250 and as follows: O -Annealed T6 -Solution-heat-treated and artificially aged. T62 -Solution-heat-treated from the O or F temper to demonstrate the response to heat- treatment, and artificially aged. T651 -Solution-heat-treated, stress relieved by stretching to produce a nominal permanent set of 2 percent but not less than 1-1/2 nor more than 3 percent, and artificially aged. Plate shall receive no further straightening after stretching. T76 -Solution-heat-treated and artificially aged sufficient to produce improved resistance to exfoliation. T7651 -Solution-heat-treated, stress relieved by stretching to produce a nominal permanent set of 2 percent but not less than 1-1/2 nor more than 3 percent, and artificially aged sufficient to produce improved resistance to exfoliation and stress corrosion cracking. Plate shall receive no further straightening after stretching. F -As fabricated.strRefField
【与前一版的变化】

替代标准

包含图表

Chemical Composition
Mechanical Propertie
Bend Test Factor "N"
Cladding Thickness
Ultrasonic Discontin
TABLE 1
SURFACE APPEARANCE O
FOUR DEGREES OF SEVE
75X - UNETCHED, STRE
75X - UNETCHED, PITT